Abstract:All solid-state lithium batteries (ASS-LBs) with polymer-based solid electrolytes are a prospective contender for the next-generation batteries because of their high energy density, flexibility, and safety. Among all-polymer electrolytes, PEO-based solid polymer electrolytes received huge consideration as they can dissolve various Li salts. However, the development of an ideal PEO-based solid polymer electrolyte is hindered by its insufficient tensile strength and lower ionic conductivity due to its semi-crystalline and soft chain structure. In order to lower the crystallization and improve the performance of PEO-based solid polymer electrolyte, tungsten trioxide (WO3) nanofillers were introduced into PEO matrix. Herein, a PEO20/LiTFSI/x-WO3 (PELI-xW) (x = 0%, 2.5%, 5%, 10%) solid composite polymer electrolyte was prepared by the tape casting method. The solid composite polymer electrolyte containing 5 wt% WO3 nanofillers achieved the highest ionic conductivity of 7.4 x 10-4 S cm-1 at 60 degrees C. It also confirms a higher Li-ion transference number of 0.42, good electrochemical stability of 4.3V, and higher tensile strength than a PEO/LiTFSI (PELI-0W) fillers-free electrolyte. Meanwhile, the LiFePO4|PELI-xW|Li ASS-LBs demonstrated high performance and cyclability. Based on these findings, it can be considered a feasible strategy for the construction of efficient and flexible PEO-based solid polymer electrolytes for next-generation solid-state batteries.
Document Type:Article
Volume:49
Issue:3
Page Number:4473-4481
ISSN No.:0272-8842
Translation or Not:no
Pre One:Ionogel electrolyte with dynamic metal-ligand interactions enabled self-healable supercapacitor with high energy density
Next One:Gradient fluorinated and hierarchical selective adsorption coating for Zn-Based aqueous battery
Release time:2025-05-23